A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy® E-14292 Hi-Flow Glass Reinforced PPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Specific Gravity 1.64 g/cc
1.64 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.175 mm
0.0020 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 215 MPa
31200 psi
ASTM D790
Flexural Modulus 14.35 GPa
2081 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 263 °C
505 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ASTM D648