Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical LB100M PVC General Description: LB100M, blend resin exhibits the following characteristics. Reduced viscosity, aging of plastisol, low gloss at the top layers and improved deaeration of plasticallyMain Applica.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical LP090 PVC General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical LP170 PVC General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical LP170G PVC General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical LP170L PVC General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for .. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PB1202 PVC General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PB1302 PVC General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PB1752 PVC General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PB900 PVC General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary .. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | |
LG Chemical PE1311 PVC General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin.. |
|||
Specific Gravity | 1.406 g/cc | 1.406 g/cc | ASTM D792 |
PolyOne Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |