Material Notes:
Features:For deep or hard to form parts where good finished detail is requiredMore rigid than most thermoplastics, parts deform less when loadedMeets highest standard for chemical resistance for thermoplastic materialsExcellent forming properties, uniform wall thicknessSuggested Applications:Aircraft InteriorsKiosk HousingsMedical HousingsExhibits and DisplaysStore FixturesOffice FurnitureInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 45.0 MPa
6530 psi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
ASTM D648
Flammability, UL94 V-0
V-0
5VA
5VA
Descriptive Properties Value Comments
Federal Aviation Administration Pass
FAR 25.853 (a)
Surface Burning Characteristics: Flame Spread/Smoke Class 1/A
ASTM E84