Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne LubriOne™ NI-30CF/15T-2S Polyamide 610 (Nylon 610)

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer PolyOne Corporation
Trade Name LubriOne™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne LubriOne™ NI-30CF/15T-2S Polyamide 610 (Nylon 610).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 172 MPa
24900 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 10.3 GPa
1490 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 221 MPa
32100 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
4.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
ASTM D257
Descriptive Properties Value Comments
Features Lubricated
Forms Pellets
Generic Material Nylon 610
Generic Name Polyamide 610 (Nylon 610)
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
Uses Appliance Components
Conveyor Parts
Printer Parts