Polymer Property : Specific Gravity = 0.963 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.955 - 0.963 g/cc

@Temperature 20.0 °C
0.955 - 0.963 g/cc

@Temperature 68.0 °F
DIN 51 757/ASTM D4052
The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester
VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined wi..