Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer The Chemical Company
Trade Name VESTINOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined with fast fusion properties makes this an ideal plasticizer for chemical foamed flooring applications. For use with PVC, PAMA, PVB etc. Plasticizing/coalescing agent for paints, inks, coatings, and adhesives.Information provided by The Chemical Company
Physical Properties Metric English Comments
Specific Gravity 0.955 - 0.963 g/cc

@Temperature 20.0 °C
0.955 - 0.963 g/cc

@Temperature 68.0 °F
DIN 51 757/ASTM D4052
Brookfield Viscosity 8.4 cP

@Temperature 20.0 °C
8.4 cP

@Temperature 68.0 °F
DIN S3015/ASTM D445
Molecular Weight 248 g/mol
248 g/mol
Vapor Pressure 2.40e-7 bar

@Temperature 20.0 °C
0.000180 torr

@Temperature 68.0 °F
OECD Testing Guideline 104
Thermal Properties Metric English Comments
Pour Point -60.0 °C
-76.0 °F
DIN ISO 3016
Flash Point 161 °C
322 °F
DIN EN ISO 2719
Optical Properties Metric English Comments
Refractive Index 1.488 - 1.494

@Temperature 20.0 °C
1.488 - 1.494

@Temperature 68.0 °F
DIN 51 423/2/ASTM D1045
Chemical Properties Metric English Comments
Acid Value <= 0.070
<= 0.070
mg KOH/g; DIN EN ISO 2114/ASTM D1045
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Percent by mass; DIN 51 777/ASTM E 203
Solution Temperature 128 °C
262 °F
DIN 54 408, modified
Descriptive Properties Value Comments
Appearance Clear and free of suspended matter
Assay = 99.7%
Degussa-Hüls
Hazen Color Value (pt-co) < 40
Mg Pt/I, DIN ISO 6271/ASTM D1209
Ignition Temp (°C) 370
DIN 51 794/ASTM E 659