Polymer Property : Specific Gravity = 0.955 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Polimeri Europa Eraclene® MS 80 U High Density Polyethylene - Injection Molding
Eraclene MS 80 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This grade has a narrow molecular weight distribution and a hig..
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding
Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro..
Specific Gravity 0.955 g/cc
0.955 g/cc
20/20°C
LyondellBasell Glycol Ether DB Diethylene glycol butyl ether
Information provided by Lyondell.
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D1238
I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade
Features:IS-35955 is designed for applications requiring excellent stiffness and stress crack resistance properties.Meets all requirements of the U. S. Food and Drug Administration as specified in 2..
Specific Gravity 0.955 - 0.958 g/cc
0.955 - 0.958 g/cc
ASTM D1505
LG Chemical SEETEC PH162 HDPE
Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Specific Gravity 0.955 g/cc
0.955 g/cc
Struktol TPW 101 Processing Additive
Mixture of zinc stearate and waxes.STRUKTOL® TPW 101 is a general-purpose blend of lubricants designed to provide improved processing characteristics of highly filled polyolefin compounds. This p..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Teknor Apex Sinpolene TPP1010 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Total HDPE HL 535 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release ..
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra..
Specific Gravity 0.955 - 0.963 g/cc

@Temperature 20.0 °C
0.955 - 0.963 g/cc

@Temperature 68.0 °F
DIN 51 757/ASTM D4052
The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester
VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined wi..
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Total XSene® 4206 B High Density Polyethylene - Steel Pipe Coating
HDPE 4206 B is a high performance black compound primarily intended for steel pipe coating applications.Key characteristics areSuperior mechanical properties under stress cracking as well as under i..
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Total XSene® 55060 High Density Polyethylene - Blow Molding
HDPE 55060 is a semi high molecular weight (SHMW) high density polyethylene with outstanding Environmental Stress Crack Resistance and rigidity. It has been specifically designed for the manufactur..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene
A natural HDPE resin, specifically designed for high speed blow molding and extrusion applications.
Specific Gravity 0.955 g/cc
0.955 g/cc
ISO 1183
Total XSene® HD55110 High Density Polyethylene - Blown Film
HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene
Copolymer Polypropylene, Unreinforced, 20 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, ..
Specific Gravity 0.955 g/cc
0.955 g/cc
23/23°C; ASTM D792
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.