PolyOne Synprene® IT 705 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® IT 705 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedOpaqueApplications:Multi-PurposeGaskets and SealsProcessing Method:ExtrusionPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
Instant; ASTM D2240
Tensile Strength, Yield 7.412 MPa
1075 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
4.69 MPa

@Strain 300 %
680 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 525 %
525 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 35.1 kN/m
200 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 18 %
18 %
Method B, 73°F(23°C), 22 hrs; ASTM D395