Polymer Property : Specific Gravity = 0.942 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.942 - 0.945 g/cc
0.942 - 0.945 g/cc
ASTM D1505
LG Chemical SEETEC PH150 HDPE Blown Film Grade
Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistanceAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 20..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM 792
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM 792
Multibase Multi-Flex® D 5308 X Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM 792
Multibase Multi-Flex® G 7430 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM 792
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
Teknor Apex Telcar® TL-88-N882-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..
Specific Gravity 0.942 g/cc
0.942 g/cc
ISO 1183
Total MDPE HR 515 Medium Density Polyethylene, Blown Film
MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..
Specific Gravity 0.942 g/cc
0.942 g/cc
ASTM D792
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from..