Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D792 |
S&E Specialty Polymers G-4285UV PVC Application: UV resistant, PVC material designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | <= 1.40 g/cc | <= 1.40 g/cc | ISO 1183, A |
S&E Specialty Polymers XP44-11 PVC Description: PVC weatherable, integral colored, filledApplication: Body side skin extrusion and injection molding compound meets GMP.PVC.015, GMP.PVC.093, GMP.PVC.094, Chrysler MSDC 543, and Ford WS.. |
|||
Specific Gravity | 1.40 - 1.50 g/cc | 1.40 - 1.50 g/cc | |
PolyChem Alloy AquaGard™ 6004 AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene .. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | (Dry) |
Radici Radiflam® S RV250FR (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 136 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy saving and the ability to work with heat sensitive substrates. The .. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ Specialty Suspension CG E 24 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E24 is a homopolymer specialty suspension resin intended for use in controlling gloss and transparency of injection molded, extruded or plastisol parts. This resin provides low surface glo.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexi.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Dry Blend E1354 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D790 |
LG Chemical LS100 PVC General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Sylvin Technologies 8980-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Colorite Polymers 9614 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Colorite Polymers 8804 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D-792 |
Axiall 9148 Wire & Cable Flexible PVC Tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Radici Radiflam® S RV250FR (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Radici Radilon® A RV350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |