Material Notes:
Geon® 136 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy saving and the ability to work with heat sensitive substrates. The vinyl ester copolymers exhibit stable Brookfield Viscosity againg characteristics. The lower molecular weight resin, Geon® 136, allows lower processing (fusion) temperature compared to Geon® 138. It provides mechanically and chemically foamable. Geon® 136 is recommended for applications where low processing temperatures are required such as carpet tile and walk off mat backings, plastisol inks, general low temperature processing applications, automotive sealants.Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 136, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 136, and 60phr DOPInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Bulk Density 0.465 g/cc
0.0168 lb/in³
Fineness 4.75
4.75
Hegman, North Fineness; Geon® 390
Relative Viscosity 2.37 cP
2.37 cP
Correlation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 4.33 cP
4.33 cP
Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
4.6 cP
4.6 cP
Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
5.55 cP
5.55 cP
One Day Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method
6.18 cP
6.18 cP
One Day Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 1.0
1.0
Inherent; ASTM D1243-60-A
Melt Flow 108 g/10 min

@Pressure 0.655 MPa
108 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
Mechanical Properties Metric English Comments
Tensile Strength 19.7 MPa
2860 psi
Optimum; With provided formulation; ASTM D638
Optical Properties Metric English Comments
Gloss 93 %
93 %
60 Degree Fused 5 mins @ 350FGeon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 93 %
93 %
Geon® ALTC 66 (with provided formulation); Internal Method
Processing Properties Metric English Comments
Moisture Content 0.050 %
0.050 %
Karl FisherGeon® STP 683; Internal Method
Descriptive Properties Value Comments
Copolymer Content 4.9%
Internal Method; Geon® STP PT-LA-026
Features Fast Fusion
Low VOC
Forms Powder
Fine, White Powder
Gel Temperature 65 °C
Internal Method; Geon® ALTC 29 (with provided formulation)
Generic Material PVC Copolymer
Generic Name Polyvinyl Chloride Copolymer (PVC Copolymer)
K-Value 70
Internal Method; Correlation, 0.5gm/100ml
Methanol Extractables 2.3%
Internal Method; Geon® STP 894
Polymerization Process Microsuspension
Processing Method Casting
Dip Coating
Rotational Molding
Slush Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Residual Vinyl Chloride Monomer < 9 ppm
Internal Method; Geon® STP 1005
Uses Automotive Applications
Carpet Backing
Sealants