Polymer Property : Brookfield Viscosity = 435000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 195000 - 435000 cP

@Temperature 25.0 °C
195000 - 435000 cP

@Temperature 77.0 °F
262 Resin; HAT-TD @ 5rpm
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive
LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi..
Brookfield Viscosity 195000 - 435000 cP

@Temperature 25.0 °C
195000 - 435000 cP

@Temperature 77.0 °F
262B Resin; HAT-TD @ 5rpm
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive
LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum..