Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 195000 - 435000 cP @Temperature 25.0 °C |
195000 - 435000 cP @Temperature 77.0 °F |
262 Resin; HAT-TD @ 5rpm |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Brookfield Viscosity | 195000 - 435000 cP @Temperature 25.0 °C |
195000 - 435000 cP @Temperature 77.0 °F |
262B Resin; HAT-TD @ 5rpm |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |