Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 4.90 cm @Load 750 kg, Temperature 320 °C |
1.93 in @Load 1650 lb, Temperature 608 °F |
0.5mm diameter |
Kuraray Genestarâ„¢ GA2330 Nylon, 33% Glass Filled Abrasion Resistance V-0 Grade. Can be used for applications requiring high abrasion and heat resistance, as well as flame retardancy, such as internal gear of copying machine. |