Physical Properties Metric English Comments
Spiral Flow 4.90 cm

@Load 750 kg,
Temperature 320 °C
1.93 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Kuraray Genestarâ„¢ GA2330 Nylon, 33% Glass Filled
Abrasion Resistance V-0 Grade. Can be used for applications requiring high abrasion and heat resistance, as well as flame retardancy, such as internal gear of copying machine.