Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 32.8 cm | 12.9 in | Equistar test |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |