Polymer Property : Spiral Flow = 12.9 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 32.8 cm
12.9 in
Equistar test
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the ..