Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the requirements of the Food and Drug Administration 21 CFR 177.1520. This regulation allows the use of this olefin polymer in” …articles or components or articles intended for use in contact with food.” Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Specific recommendations for processing GA564189 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Spiral Flow 32.8 cm
12.9 in
Equistar test
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Tensile Strength, Yield 13.8 MPa
2000 psi
20"/min; ASTM D638
Elongation at Yield 12 %
12 %
20"/min; ASTM D638
1% Secant Modulus 379 MPa
55000 psi
0.5"/min; ASTM D790
2% Secant Modulus 0.317 GPa
46.0 ksi
0.5"/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C
117 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<SUB>50</SUB>; ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 177 °C
350 °F
Middle Barrel Temperature 191 °C
375 °F
Front Barrel Temperature 204 °C
400 °F
Nozzle Temperature 204 °C
400 °F