Polymer Property : Spiral Flow = 32.0 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 32.0 cm
12.6 in
Equistar
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder..
Spiral Flow 32.0 cm
12.6 in
Melt temperature at 330°C; Spiral mold 1.5 x 6 mm; 17 mm for 10MFR PC resins
LG Chemical Lupoy 3010-30 Polycarbonate Resin
Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Spiral Flow 32.0 - 67.8 cm
12.6 - 26.7 in
Average value: 47.6 cm Grade Count:10
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..