Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 33.0 - 41.0 cm | 13.0 - 16.1 in | Average value: 36.3 cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |