Physical Properties Metric English Comments
Spiral Flow 33.0 - 41.0 cm
13.0 - 16.1 in
Average value: 36.3 cm Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Spiral Flow 33.0 cm
13.0 in
Exxon Method
ExxonMobil Escorene® HD-6704 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCRUses: Industrial containers, Industrial lids
Spiral Flow 33.0 cm

@Pressure 27.6 MPa,
Temperature 163 °C
13.0 in

@Pressure 4000 psi,
Temperature 325 °F
Mesa
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert..
Spiral Flow 33.0 cm
13.0 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
LyondellBasell Alathon® H5618 High Density Polyethylene
ApplicationsALATHON H 5618 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inc..