Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 35.0 - 700 cm | 13.8 - 276 in | Average value: 110 cm Grade Count:10 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Spiral Flow | 35.0 - 45.0 cm | 13.8 - 17.7 in | Average value: 41.3 cm Grade Count:8 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Spiral Flow | 35.1 cm | 13.8 in | Equistar test |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |
|||
Spiral Flow | 35.0 cm | 13.8 in | Cross Section: 7[mm]x3.5[mm]; AKRO |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Spiral Flow | 35.0 cm | 13.8 in | AKRO |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Spiral Flow | 35.0 - 107 cm | 13.8 - 42.1 in | Average value: 77.5 cm Grade Count:11 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |