Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 35.0 - 107 cm | 13.8 - 42.1 in | Average value: 77.5 cm Grade Count:11 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |