Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00090 cm/cm
0.00090 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00090 cm/cm
0.00090 in/in
SABIC Method
SABIC Innovative Plastics LNP Stat-kon ZEL34XXC PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZEL34XXC is a compound based on PPE+PS Blend resin containing Carbon Fiber, PTFE. Added features include : Electrically Conductive , Internally Lubricated.This data was supplied by S..
Linear Mold Shrinkage, Flow 0.00090 cm/cm
0.00090 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
Linear Mold Shrinkage, Flow 0.00090 - 0.020 cm/cm

@Time 86400 sec
0.00090 - 0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK
LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu..
Linear Mold Shrinkage, Flow 0.00090 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00090 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Linear Mold Shrinkage, Flow 0.00090 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00090 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Linear Mold Shrinkage, Flow 0.00090 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00090 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Linear Mold Shrinkage, Flow 0.00090 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00090 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Linear Mold Shrinkage, Flow 0.00090 cm/cm
0.00090 in/in
Compression molding; ISO 2577
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength  (discontinued **)
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p..