Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.800 g/cc @Temperature 15.5 °C |
0.800 g/cc @Temperature 59.9 °F |
|
Indium Corp. 3577-TF Wave Solder Flux, No-Clean Wave Solder Flux 3577-TF is a low-solids flux specially formulated to eliminate post-cleaning operations. This flux contains a small amount of resin, which enhances the wetting properties.3577-TF i.. |
|||
Specific Gravity | 0.800 g/cc @Temperature 25.0 °C |
0.800 g/cc @Temperature 77.0 °F |
|
Indium Corp. 3541 Wave Solder Flux, No-Clean 3541 No-Clean is a low-solids flux specially formulated to be used for wave soldering where the cleaning process has been eliminated. This flux contains a small amount of resin which enhances the w.. |