Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 3541 Wave Solder Flux, No-Clean

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 3541 Wave Solder Flux, No-Clean.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3541 No-Clean is a low-solids flux specially formulated to be used for wave soldering where the cleaning process has been eliminated. This flux contains a small amount of resin which enhances the wetting properties.3541 No-Clean is activated by a multi-component, synergetic fluxing system, which improves solderability. Any post-soldering residues are considered non-corrosive.3541 No-clean leaves a "tack-free" surface and does not interfere with ATE testing.Features:Eliminates the need for cleaningReduces solder ball formationExcellent solderability on standard board finishes and alternative coatingPhysical Properties Color: StrawJ-STD-004 Flux Type: ORL0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.800 g/cc

@Temperature 25.0 °C
0.800 g/cc

@Temperature 77.0 °F
0.806 g/cc

@Temperature 15.5 °C
0.806 g/cc

@Temperature 59.9 °F
Solids Content 4.31 %
4.31 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Electrical Properties Metric English Comments
Insulation Resistance 1.88e+13 ohm
1.88e+13 ohm
Control - final; Standard Bellcore
2.68e+13 ohm
2.68e+13 ohm
Control - initial; Standard Bellcore
3.76e+9 ohm

@Time 605000 sec
3.76e+9 ohm

@Time 168 hour
Control; IPC B25A
1.74e+10 ohm

@Time 86400 sec
1.74e+10 ohm

@Time 24.0 hour
Control; IPC B25A
Chemical Properties Metric English Comments
Acid Value 25
25
Users viewing this material also viewed the following: