Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.040 - 0.060 cm/cm | 0.040 - 0.060 in/in | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead ML11 General Grade BOPP Matt Film (thickness: 15 µm) ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board laminati.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead ML11 General Grade BOPP Matt Film (thickness: 30 µm) ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board laminati.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead ML21 General Grade BOPP Matt Film (thickness: 15 µm) ML21 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. Both sides have corona treatment. It is specially designed for board lamin.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead ML21 General Grade BOPP Matt Film (thickness: 20 µm) ML21 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. Both sides have corona treatment. It is specially designed for board lamin.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead ML21 General Grade BOPP Matt Film (thickness: 30 µm) ML21 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. Both sides have corona treatment. It is specially designed for board lamin.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 50 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 25 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 40 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 50 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 50 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 40 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 18 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 12 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 20 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 18 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 30 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 35 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 18 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 20 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | ASTM-D1204 |
Kinlead PP11 Printing Grade BOPP Plain Film (thickness: 30 µm) PP11 is a general, printing grade BOPP plain film. It is transparent and non heat sealable. It has excellent ink adhesion. One side has corona treatment. It is widely used in printing applications.I.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Linear Mold Shrinkage | 0.040 cm/cm | 0.040 in/in | |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Linear Mold Shrinkage | 0.040 - 0.060 cm/cm | 0.040 - 0.060 in/in | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |