Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | cylinder; per Dyneon method |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 20 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm) PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ Electro 242-15 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2003 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2631 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2725/40 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3786/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 30 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2328 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |