Material Notes:
Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.820 g/cc
0.0296 lb/in³
DIN 53 466
Linear Mold Shrinkage 0.035 cm/cm
0.035 in/in
cylinder; per Dyneon method
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
Sintered molding, DIN 53 505
Tensile Strength, Ultimate 33.0 MPa

@Thickness 0.200 mm
4790 psi

@Thickness 0.00787 in
Sintered moldings; ASTM D4894/4895
Elongation at Break 560 %
560 %
Sintered Molding; ASTM D4894
Tensile Modulus 0.650 GPa
94.3 ksi
Sintered Molding, DIN 53457
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C

@Temperature 30.0 - 100 °C
66.7 µin/in-°F

@Temperature 86.0 - 212 °F
140 µm/m-°C

@Temperature 30.0 - 200 °C
77.8 µin/in-°F

@Temperature 86.0 - 392 °F
170 µm/m-°C

@Temperature 30.0 - 300 °C
94.4 µin/in-°F

@Temperature 86.0 - 572 °F
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52 612
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service Temp
Minimum Service Temperature, Air -200 °C
-328 °F
Continuous Service Temp
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
IEC 60093
Dielectric Strength 65.0 kV/mm
1650 kV/in
200µm film; IEC 60243-1