PlastxWorld Veroplas PB2009L Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PB2009L Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
general purpose, unfilled, lubricated injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.028 cm/cm
0.028 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 77.9 MPa
11300 psi
ASTM D638
Elongation at Break 18 %
18 %
ASTM D638
Flexural Yield Strength 95.1 MPa
13800 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 199 °C
390 °F
ASTM D1525
Glow Wire Test 649 °C
1200 °F
UNE 20-672-83