Physical Properties Metric English Comments
Linear Mold Shrinkage 0.011 - 0.0125 cm/cm

@Thickness 3.17 mm
0.011 - 0.0125 in/in

@Thickness 0.125 in
Ovation Polymers Nima™ NH PA66UT Nylon 66
Polyamide 66 - Ultra Tough, Flame Retarded Non-Hal grade with excellent retention of mechanical properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humi..
Linear Mold Shrinkage 0.011 - 0.0125 cm/cm

@Thickness 3.17 mm
0.011 - 0.0125 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66UT108 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Linear Mold Shrinkage 0.011 - 0.0125 cm/cm

@Thickness 3.17 mm
0.011 - 0.0125 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66UT119 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Linear Mold Shrinkage 0.000500 - 0.0125 cm/cm
0.000500 - 0.0125 in/in
Average value: 0.00805 cm/cm Grade Count:21
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..