Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0053 cm/cm | 0.0053 in/in | ASTM D955 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Linear Mold Shrinkage | 0.0053 cm/cm | 0.0053 in/in | ASTM D955 |
Plenco 3557 Phenolic, Granular, Compression Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Linear Mold Shrinkage | 0.0053 cm/cm | 0.0053 in/in | ASTM D955 |
Plenco 4527 Phenolic, Granular, Injection Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |
|||
Linear Mold Shrinkage | 0.0053 - 0.0059 cm/cm | 0.0053 - 0.0059 in/in | ASTM D955 |
Buckeye Polymers BP FLEX D6520 T BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |