Plenco 4527 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4527 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under component file E40654. 04527 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
ASTM D1895
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0053 cm/cm
0.0053 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 57
57
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 0.85 %
0.85 %
ASTM D638
Tensile Modulus 10.1 GPa
1460 ksi
ASTM D638
Flexural Strength 79.0 MPa
11500 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Compressive Strength 139 MPa
20200 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM D638
Shear Modulus 3.77 GPa
547 ksi
Calculated
Izod Impact, Notched 0.190 J/cm
0.356 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.205 J/cm²
0.976 ft-lb/in²
ASTM D256
Impact 144
144
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 34.0 µm/m-°C

@Temperature 40.0 - 130 °C
18.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.550 W/m-K

@Temperature 100 °C
3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 202 °C
396 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 31 %
31 %
ASTM D2863
Shrinkage 0.34 %
0.34 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+12 ohm-cm
1.70e+12 ohm-cm
ASTM D247
Dielectric Constant 6.5
6.5
ASTM D150
Dielectric Strength 7.30 kV/mm
185 kV/in
Step by Step; ASTM D149
9.40 kV/mm
239 kV/in
Short Time; ASTM D149
Dissipation Factor 0.162
0.162
ASTM D150
Arc Resistance 181 sec
181 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638