Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0047 cm/cm | 0.0047 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 49 GF 20 Polypropylene Homopolymer, 20% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.0047 cm/cm | 0.0047 in/in | Isotropy |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
Linear Mold Shrinkage | 0.0047 cm/cm | 0.0047 in/in | ASTM D955 |
Teknor Apex Sinpolene GPP1615/2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 15% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Linear Mold Shrinkage | 0.0047 cm/cm | 0.0047 in/in | ASTM D955 |
Plenco 2300 Phenolic, Granular, Compression Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Linear Mold Shrinkage | 0.0047 cm/cm | 0.0047 in/in | |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |