Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fiberglass and 25% mineral filling, high-strength mechatronic plastic parts can be manufactured efficiently, quickly and flexibly with LDS. The innovative material offers a broad processing window for optimal results regarding: laser activation, metallization, adhesion of the conductors. Ultramid T 4381 LDS is based on Ultramid T and offers an ideal combination of high melting temperature, good processability and low water absorption. This specialty from BASF’s engineering plastics is already being used in electrical engineering and automotive construction, especially where high heat distortion temperature is required.Information provided by BASF
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Water Absorption 4.2 - 5.2 %
4.2 - 5.2 %
ISO 62
Moisture Absorption at Equilibrium 0.80 - 1.2 %
0.80 - 1.2 %
50% RH; ISO 62
Viscosity Measurement 130
130
ISO 307
Linear Mold Shrinkage 0.0047 cm/cm
0.0047 in/in
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 265 °C
509 °F
ISO 75-2
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+12 ohm-cm
3.00e+12 ohm-cm
IEC 60093
Dielectric Constant 4.2

@Frequency 1.00e+6 Hz
4.2

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.038

@Frequency 1.00e+6 Hz
0.038

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Melt Temperature 310 - 330 °C
590 - 626 °F
Injection molding/Extrusion
Mold Temperature 100 - 140 °C
212 - 284 °F
Injection molding
Descriptive Properties Value Comments
Color Black
Commercial Status Europe