Polymer Property : Linear Mold Shrinkage = 0.00350 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00100 - 0.00350 cm/cm
0.00100 - 0.00350 in/in
Average value: 0.00275 cm/cm Grade Count:5
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Linear Mold Shrinkage 0.000600 - 0.00350 cm/cm
0.000600 - 0.00350 in/in
Average value: 0.00197 cm/cm Grade Count:23
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..