Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3509 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3509 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file E40654. 03509 is available in black or brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.169 %
0.169 %
ASTM D570
Linear Mold Shrinkage 0.00281 cm/cm
0.00281 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 84
84
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 0.60 %
0.60 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
Compressive Strength 194 MPa
28100 psi
ASTM D695
Izod Impact, Notched 0.199 J/cm
0.373 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ASTM D256
Impact 117
117
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C

@Temperature 40.0 - 130 °C
32.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.470 W/m-K

@Temperature 100 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 204 °C
399 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 194 °C
381 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 38 %
38 %
ASTM D2863
Shrinkage 0.086 %
0.086 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.30e+12 ohm-cm
3.30e+12 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 14.4 kV/mm
366 kV/in
Step by Step; ASTM D149
17.4 kV/mm
442 kV/in
Short Time; ASTM D149
Dissipation Factor 0.0274
0.0274
ASTM D150
Arc Resistance 172 sec
172 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638