Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0018 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ASTM D955
North Wood Plastics Polypropylene with 60% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ASTM D955
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ISO 2577
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP
BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ISO 2577
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP
BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories ..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ISO 2577
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound
Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
E-Polymers SEPAZ® LA50 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
E-Polymers SEPAZ® LB50 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
24 hrs; ISO 294
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled  (discontinued **)
LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat..
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ATM D955
Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform..
Copyright © lookpolymers.com All Rights Reserved