Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ASTM D955 |
North Wood Plastics Polypropylene with 60% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ASTM D955 |
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ISO 2577 |
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage.. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ISO 2577 |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ISO 2577 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | |
E-Polymers SEPAZ® LA50 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | |
E-Polymers SEPAZ® LB50 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | 24 hrs; ISO 294 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |
|||
Linear Mold Shrinkage | 0.0018 cm/cm | 0.0018 in/in | ATM D955 |
Plenco 50335 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |