Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0018 cm/cm
0.0018 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120.5 MPa
17480 psi
ASTM D638
Elongation at Break 1.81 %
1.81 %
ASTM D638
Tensile Modulus 9.47 GPa
1370 ksi
ASTM D638
Flexural Yield Strength 179.3 MPa
26010 psi
ASTM D790
Flexural Modulus 9.04 GPa
1310 ksi
ASTM D790
Compressive Yield Strength 172.7 MPa
25050 psi
ASTM D695
Izod Impact, Notched 0.560 J/cm
1.05 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 224 °C
435 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
424 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.96e+17 ohm-cm
3.96e+17 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.3 kV/mm
439 kV/in
Short Time; ASTM D149
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 70 sec
70 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
ASTM D3638
Users viewing this material also viewed the following: