Polymer Property : Fiber Count = 17.0 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 14.0 - 17.0 dtex
12.6 - 15.3 denier
EMS-Griltech Grilon® TN 5000 White Nylon 6 Fiber
Description: GRILON TN 5000 is a non-set fiber with high shrinkage which is used for special press felt applications.Data provided by EMS-Griltech.
Fiber Count 6.70 - 17.0 dtex
6.03 - 15.3 denier
EMS-Griltech Grilon® TS 5021 White Nylon 6 Fiber
Description: GRILON TS 5021 is a super-set fiber with very good recovery. It is used as a construction element for press felts.Data provided by EMS-Griltech.