Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 14.0 - 17.0 dtex | 12.6 - 15.3 denier | |
EMS-Griltech Grilon® TN 5000 White Nylon 6 Fiber Description: GRILON TN 5000 is a non-set fiber with high shrinkage which is used for special press felt applications.Data provided by EMS-Griltech. |
|||
Fiber Count | 6.70 - 17.0 dtex | 6.03 - 15.3 denier | |
EMS-Griltech Grilon® TS 5021 White Nylon 6 Fiber Description: GRILON TS 5021 is a super-set fiber with very good recovery. It is used as a construction element for press felts.Data provided by EMS-Griltech. |