EMS-Griltech Grilon® TS 5021 White Nylon 6 Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® TS 5021 White Nylon 6 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON TS 5021 is a super-set fiber with very good recovery. It is used as a construction element for press felts.Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 22.0 - 44.0 dtex
19.8 - 39.6 denier
Descriptive Properties Value Comments
Color Raw White
Crimp High
Luster Bright
Staple Length 97 mm