Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil Exceed™ 1518KC Metallocene Polyethylene Resin Product Description: Exceed 1518KC is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518KC have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Slip Level | 800 ppm | 800 ppm | |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |