Polymer Property : Molecular Weight = 6500 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 6500 g/mol
6500 g/mol
Westlake Epolene® N-21 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-21 is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity m..
Molecular Weight 6500 g/mol
6500 g/mol
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier..
Molecular Weight 6500 g/mol
6500 g/mol
BASF Pluracol® 2100 Slabstock HR Foam Polyol
Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Plurac..
Molecular Weight 6500 g/mol
6500 g/mol
BASF Pluracol® 380 Specialty Polyol
Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation..