Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 50000 g/mol | 50000 g/mol | |
Lucite International Elvacite ® 2043 Acrylic Resin Elvacite® 2043 is a low molecular weight ethyl methacrylate copolymer. It is a fast – dissolving, low viscosity resin with alcohol solubility for flexographic inks. Most compatible grade. It.. |
|||
Molecular Weight | >= 50000 g/mol | >= 50000 g/mol | |
Sichuan Deyang Haton® hd Polyphenylene Sulfide Resin Film gradeInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Molecular Weight | 50000 g/mol | 50000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® US130J Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Molecular Weight | 50000 g/mol | 50000 g/mol | ASTM D3536 |
SK Chemicals SKYTHANE® US230 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |