SK Chemicals SKYTHANE® US130J Ink Binder

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® US130J Ink Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets and FilmHoses and TubingShoe ComponentsFire HosesInformation provided by SK Chemicals.
Physical Properties Metric English Comments
Solids Content 40 %
40 %
ASTM D1259
Viscosity 40000 - 80000 cP
40000 - 80000 cP
ASTM D803
Molecular Weight 50000 g/mol
50000 g/mol
ASTM D3536
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.7 MPa
2280 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
100% Modulus 0.00157 GPa
0.228 ksi
ASTM D638
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -5.00 °C
23.0 °F
ASTM E1356
Descriptive Properties Value Comments
Appearance Pale Yellow Liquid