Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Elvacite ® 2043 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2043 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2043 is a low molecular weight ethyl methacrylate copolymer. It is a fast – dissolving, low viscosity resin with alcohol solubility for flexographic inks. Most compatible grade. It provides excellent pigment wetting ability and broad solubility for use in lacquers for solvent – sensitive substrates.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Particle Size 140 - 220 µm
140 - 220 µm
Viscosity Measurement 0.18 - 0.238
0.18 - 0.238
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 50000 g/mol
50000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 11
11
Tukon Hardness
Tensile Strength 6.89 MPa
999 psi
Elongation at Break 0.60 %
0.60 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 66.0 °C
151 °F
Chemical Properties Metric English Comments
Total Acid Number 8.0
8.0
Processing Properties Metric English Comments
Moisture Content 0.60 %
0.60 %
Users viewing this material also viewed the following: