Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 4800 g/mol | 4800 g/mol | |
BASF Pluracol® 2097 Molded Foam Polyol Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with.. |
|||
Molecular Weight | 4800 g/mol | 4800 g/mol | |
BASF Pluracol® 816 Molded Foam Polyol Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol .. |
|||
Molecular Weight | 4800 g/mol | 4800 g/mol | |
BASF Pluracol® 1421 Molded Foam Polyol Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol.. |