Polymer Property : Molecular Weight = 4800 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 4800 g/mol
4800 g/mol
BASF Pluracol® 2097 Molded Foam Polyol
Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with..
Molecular Weight 4800 g/mol
4800 g/mol
BASF Pluracol® 816 Molded Foam Polyol
Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol ..
Molecular Weight 4800 g/mol
4800 g/mol
BASF Pluracol® 1421 Molded Foam Polyol
Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol..